Related Experiment Video
Updated: Feb 24, 2026

Solid-state Graft Copolymer Electrolytes for Lithium Battery Applications
Published on: August 12, 2013
Aluminum Acetylacetonate-Confined In-Situ Polymer as Dynamic Active Medium for Sustainable Solid-State Lithium-Sulfur
Yi Zhang1, Wenyi He1, Hun Kim2
1Key Lab for Special Functional Materials of Ministry of Education, National & Local Joint Engineering Research Center for High-efficiency Display and Lighting Technology, School of Nano Science and Materials Engineering, Collaborative Innovation Center of Nano Functional Materials and Applications, Henan University, Kaifeng 475004, China.
Abstract:
Solid polymer electrolyte (SPE)-based lithium-sulfur (Li-S) batteries attract significant interest due to their high theoretical energy densities and enhanced safety profiles. However, the clogging of the cathode-SPE interface with ″dead″ lithium polysulfide (LiPS) is the core failure mechanism of the SPE-based Li-S battery. This induces a sluggish, irreversible electrochemical environment, hindering redox processes and limiting the practical implementation of high-energy-density solid-state Li-S batteries (SSLSBs). To address this problem, this study proposes the generation of a dynamic active medium (DAM) electrolyte system at the cathode interface. Based on the coordination effect between aluminum acetylacetonate and 1,3-dioxolane (DOL), this system is introduced between the cathode and in situ-polymerized polyDOL-based SPE, synergistically realizing three functions: (1) optimizing the electrode-electrolyte interfacial compatibility, (2) adsorbing and reactivating the LiPS accumulated at the interface, and (3) reducing the energy barriers of the S redox reactions and accelerating the sulfide conversion kinetics. This approach enables the SSLSB to reach a high energy density of 347 Wh kg-1 at a high S loading of 4.5 mg cm-2. The pouch cell configuration maintains a capacity retention rate as high as 85.3% after 80 cycles. Moreover, this interfacial DAM strategy provides an innovative engineering concept to suppress the accumulation of LiPS in SSLSBs.
Related Concept Videos
Weak Acid Solutions
Acid Halides to Alcohols: LiAlH4 Reduction
The mechanism proceeds in three steps. First, the nucleophilic hydride ion attacks the carbonyl carbon of the acid halide to form a tetrahedral intermediate. Next, the carbonyl group is re-formed, and the halide ion departs as a leaving group, generating an aldehyde. A second nucleophilic attack by the hydride yields an alkoxide ion, which, upon protonation, gives a primary alcohol as...