Evaluation of alkali residue-stabilized soil in road construction with optimization of mechanical properties and

Jing Hua1, Wenyi Xie1, Guangxia Liu1

  • 1Nanjing Institute of Environmental Science, Ministry of Ecology and Environment of China, Nanjing, China.

Plos One
|March 13, 2026
PubMed

Related Concept Videos

Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...
683
Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
651
Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
323
Quality of Water01:19

Quality of Water

In concrete preparation, the quality of water is paramount as it affects the strength and durability of the concrete. Potable water is usually preferred; however, it must not have excessive sodium or potassium to prevent compromising the concrete's integrity. Water quality is typically evaluated based on impurities such as dissolved solids, chlorides, and sulfates, and its pH value is ideally between 6 and 8. Even slightly acidic natural water may be acceptable unless it contains harmful...
630
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
435
Pozzolans01:21

Pozzolans

Pozzolans are siliceous or aluminous materials blended with Portland cement. They interact with the calcium hydroxide produced during the hydration of Portland cement and contribute to improved strength and durability of concrete. The pozzolanic activity, a measure of a pozzolan's effectiveness, is typically assessed using the strength activity index, as defined in ASTM C 618-93, which calculates the ratio of the compressive strength of cement mixtures with and without pozzolan.
Fly ash is...
666