Low-Temperature Plasma-Enhanced Atomic Layer Deposition of Cu Films Using Liquid Copper Precursor

Akihiro Nishida1,2, Atsushi Yamashita1, Masaki Enzu1

  • 1Semiconductor Materials Development Laboratory, ADEKA Corporation, 7-2-34 Higashiogu, Arakawa-ku, Tokyo 116-8553, Japan.

ACS Omega
|June 1, 2026
PubMed

Related Concept Videos

Inductively Coupled Plasma Atomic Emission Spectroscopy: Principle01:19

Inductively Coupled Plasma Atomic Emission Spectroscopy: Principle

Inductively coupled plasma (ICP) is the most widely used plasma source in atomic emission spectroscopy (AES), also known as Inductively Coupled Plasma Optical Emission Spectroscopy (ICP-OES). The ICP source, or torch, consists of three concentric quartz tubes with argon gas flowing through them. A spark from a Tesla coil initiates the ionization of argon, generating a high-temperature plasma.
The ions and electrons produced interact with the fluctuating magnetic field created by a water-cooled...
Electrodeposition01:08

Electrodeposition

Electrodeposition is a technique used to separate an analyte from interferents by electrochemical processes. Here, the analyte is a metal ion that can be deposited on an electrode immersed in the sample solution. The electrochemical setup consists of an anode and a cathode. When an electric current is applied to the setup, oxidation occurs at the anode. At the cathode, which consists of a large metal surface, metal ions undergo reduction and deposit onto the surface.
Electrodeposition can...
Preparation of Samples for Electron Microscopy01:20

Preparation of Samples for Electron Microscopy

To be visualized by an electron microscope, either transmission or scanning, biological samples need to be fixed (stabilized) so the electron beam does not destroy them and dried thoroughly (desiccated/dehydrated) so the vacuum does not affect them. Fixation needs to be done as quickly as possible because the sample properties will start changing as soon as it is removed from its natural environment. For example, in a tissue sample, the oxygen levels begin decreasing, causing an altered...