Investigation of Temperature-Field Evolution and Microstructural Response in Bituminous Waterproofing Membranes Under

Jun Tan1, Lei Geng2, Dong Zhang3

  • 1China Electronics Engineering Design Institute Co., Ltd., Beijing 100142, China.

Polymers
|June 12, 2026
PubMed

Related Concept Videos

Masonry in Cold and Hot Weather Conditions01:21

Masonry in Cold and Hot Weather Conditions

In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units and sand dry and...
Cold Weather Concreting01:27

Cold Weather Concreting

When freshly poured concrete is exposed to freezing temperatures before it has set, the water within the concrete can freeze. This expansion disrupts the setting process, delays chemical reactions necessary for hardening, and increases the volume of pores within the hardened concrete, which weakens its overall structure. If the concrete manages to reach an appreciable strength before it freezes, the damage can be somewhat mitigated.
To counteract the negative impacts of cold weather, ensuring...
Thermal Strain01:19

Thermal Strain

Thermal strain is a concept that arises when we consider how temperature changes affect structures. Unlike the conventional assumption that structures remain constant under load, real-world scenarios often involve temperature fluctuations that can significantly impact these structures. Consider a homogeneous rod with a uniform cross-section resting freely on a flat horizontal surface. If the rod's temperature increases, the rod elongates. This elongation is proportional to the temperature...
Thermal Stress01:09

Thermal Stress

If the temperature of an object is changed while it is prevented from expanding or contracting, the object is subjected to stress. The stress is compressive if the object expands in the absence of constraint and tensile if it contracts. This stress resulting from temperature change is known as thermal stress. It can be quite large and can cause damage. To avoid this stress, engineers may design components so they can expand and contract freely. For instance, on highways, gaps are deliberately...
Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
Responses to Heat and Cold Stress02:45

Responses to Heat and Cold Stress

Every organism has an optimum temperature range within which healthy growth and physiological functioning can occur. At the ends of this range, there will be a minimum and maximum temperature that interrupt biological processes.