Related Experiment Video
Updated: Jul 10, 2026

Protocol for Measuring the Thermal Properties of a Supercooled Synthetic Sand-water-gas-methane Hydrate Sample
Published on: March 21, 2016
Macro- and micro-scale mechanical properties and energy evolution analysis during unidirectional freeze-thaw cycling
Jiaming Liu1, Baoping Xi2, Yongjiang Yu3
1School of Mining Engineering, Taiyuan University of Technology, Shanxi, 030000, China.
Abstract:
This study investigates the microstructural effects, energy evolution, and damage progression of sandstone under uniaxial cyclic freeze-thaw (F-T) conditions. Using the roof sandstone from Shuangma No. 1 Mine, uniaxial compression tests were performed on samples subjected to varying numbers of F-T cycles. PFC3D simulations were employed to reproduce the failure process and analyze microcrack evolution.Results show that both the compressive strength and elastic modulus of sandstone decrease with increasing F-T cycles. When loaded perpendicular to the freeze-thaw direction, the elastic modulus of sandstone is significantly higher than that under parallel loading; conversely, the peak strain and compressive strength show the opposite trend. Post-failure analysis reveals an increase in the total number of cracks, tensile cracks, and shear cracks with more F-T cycles for both loading directions. However, the total and tensile crack counts in the parallel direction remain consistently higher than in the perpendicular direction.Energy analysis indicates that the proportion of elastic energy at peak stress continuously decreases with more F-T cycles, though it remains higher in the parallel direction. A rebound occurs at 140 cycles. The cumulative elastic energy ratio also decreases with increasing cycles, with the parallel direction consistently exhibiting higher values. Damage evolution equations, derived from the principle of minimum energy dissipation, show that the damage threshold in the parallel direction continuously increases and stays higher than in the perpendicular direction, where it first decreases and then increases. Final damage values in both directions initially rise and then decline, with transition points at 140 and 110 cycles, respectively. These findings provide theoretical guidance for rock engineering in cold regions.
More Related Videos
09:00Visualization of Failure and the Associated Grain-Scale Mechanical Behavior of Granular Soils under Shear using Synchrotron X-Ray Micro-Tomography
Published on: September 29, 2019
10:36Stress Distribution During Cold Compression of Rocks and Mineral Aggregates Using Synchrotron-based X-Ray Diffraction
Published on: May 20, 2018
Related Concept Videos
Unsoundness of Aggregate due to Volume Change
Frost Resistant Concrete
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of entrained...
Frost Action on Concrete
This freeze-thaw cycle primarily causes surface scaling, where...
Microcracking in Concrete
Fatigue
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...