Integrated Time- and Frequency-Domain Reflectometry for Non-Invasive Moisture Monitoring in Historic Masonry

Giuseppe Cannazza1, Andrea Cataldo2, Raissa Schiavoni2

  • 1Institute of Heritage Science (National Research Council), 73100 Lecce, Italy.

Related Concept Videos

Masonry in Cold and Hot Weather Conditions01:21

Masonry in Cold and Hot Weather Conditions

In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units and sand dry and...
Attenuated Total Reflectance (ATR) Infrared Spectroscopy: Overview01:13

Attenuated Total Reflectance (ATR) Infrared Spectroscopy: Overview

Attenuated total reflectance (ATR) infrared spectroscopy is a powerful analytical technique used to study the composition of materials. It is widely employed in chemistry, materials science, forensic science, and other fields where sample characterization is required. ATR has several advantages over traditional transmission IR spectroscopy, including the requirement of little to no sample preparation and the ability to analyze a wide range of samples.
The ATR process begins by directing a beam...
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
Efflorescence in Masonry01:25

Efflorescence in Masonry

Efflorescence in masonry walls appears as a fluffy crystalline powder, often white, resulting from water-soluble salts within the masonry or mortar. When water penetrates the masonry, it dissolves these salts and brings them to the surface, where they are deposited upon evaporation of water.
While initial efflorescence is common post-construction and can be cleaned with water and a brush, in certain instances, efflorescence can reappear and gradually diminish over time as salts are leached out...
Mortar Joints in Brick Masonry01:25

Mortar Joints in Brick Masonry

Mortar joints play a critical role in brick masonry, filling the spaces between brick to bind them together and provide structural integrity and strength. The thickness of these joints is variable, typically ranging from less than one-fourth inch to over half an inch, based on structural needs and specific applications.
The process of joint tooling is implemented as the mortar begins to harden. This technique involves compacting and shaping the mortar to enhance both the appearance and the...
Thermal Insulation in Masonry Walls01:22

Thermal Insulation in Masonry Walls

In hot, dry climates, the thermal mass of masonry walls can be beneficial, absorbing heat during the day and releasing it at night, thereby stabilizing indoor temperatures. However, in most other climates, additional insulation is necessary to enhance thermal resistance.
External insulation can be applied using an Exterior Insulation and Finish System (EIFS), which involves affixing panels of plastic foam to the wall and covering them with a polymeric stucco reinforced with glass fiber mesh.