Abstract:
All the vented samples with sprue widths of 2 mm or more were defect free, whereas the corresponding unvented samples had extensive voids and porosity in all but one casting. All castings with a sprue width of 1 mm were defective regardless of whether or not vents were used. The thickness of the investment above the pattern had no effect on casting results.