Related Experiment Video
Updated: Aug 18, 2026

Shrinkage of Dental Composite in Simulated Cavity Measured with Digital Image Correlation
Published on: July 21, 2014
Shear bond strength of resin composite to Dicor treated with 4-META
1Comprehensive Dentistry, Naval Dental School, Bethesda, Maryland.
Abstract:
The combination of Etch-Free Primer and C&B Metabond has been reported to produce high resin composite to feldspathic porcelain bond strengths without hydrofluoric acid etching. This study compared the shear bond strength of resin composite to a castable glass ceramic that was treated with either Etch-Free Primer and C&B Metabond or ammonium bifluoride (NH5F2) etch/silane under various surface treatment and thermal stress variables. Bond strengths after Etch-Free Primer/C&B Metabond treatment were significantly lower than those for NH5F2/silane treatment. Thermocycling was the most important variable in reducing Etch-Free Primer/C&B Metabond bond strengths.
More Related Videos
05:30Roughness Impact of Piezoelectric Dental Scaler on Two Distinct Flowable Composite Filling Materials
Published on: January 10, 2025
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024