Effects of oxalate on dentin bonding
Related Experiment Video
Updated: Nov 8, 2026

Standardized Protocol to Evaluate the Effect of Surface Treatments, Luting Cements, and Thermocycling on PEEK–Composite Bond Strength
Published on: June 9, 2026
E L Pashley1, L Tao, D H Pashley
1Department of Oral Biology/Physiology, School of Dentistry, Medical College of Georgia, Augusta, 30912-1129.
Abstract:
The purpose of this study was to determine how much topical treatment of dentin with potassium oxalate would interfere with subsequently placed dentin bonding resins. The results indicated that oxalate lowered the bond strengths of Superbond, All Bond and Scotchbond 2, but that normal bond strengths could be obtained for Superbond and All Bond after pumicing the oxalate-treated dentin.
Related Concept Videos
EDTA: Auxiliary Complexing Reagents
Complexometric Titration: Ligands
Factors Affecting Solubility
EDTA: Chemistry and Properties
Oxidations of Aldehydes and Ketones to Carboxylic Acids
Aldehydes readily undergo oxidation in strong oxidizing agents such as potassium permanganate and chromic acid. The oxidation can also be carried out using mild oxidizing agents such as silver oxide. In fact, aldehydes can be easily oxidized...
Oxidation of Alkenes: Syn Dihydroxylation with Potassium Permanganate