Related Experiment Video
Updated: Aug 13, 2026

Preparation of Extracellular Matrix Protein Fibers for Brillouin Spectroscopy
Published on: September 15, 2016
Piezoelectric and related properties of hydrated collagen
Abstract:
Two piezoelectric constants (polarization per unit stress, d=d'-id'', and polarization per unit strain, e=e'-ie''), the elastic constant, and dielectric constant are determined for oriented collagen at different hydration levels at 10 Hz from -150 to 50 degrees C. With no hydration (approximately 0% H2O), d' increases slightly with higher temperatures, while e' decreases slightly. Near 11 wt% H2O, both d' and e' increase then decrease around 0 degrees C, and is probably caused by an increase of the dielectric constant and the ionic conductivity in the nonpiezoelectric phase. Hydration greater than 25 wt%, d' and e' decrease above -50 degrees C which is considered to be due to a greater ionic conductivity surrounding the piezoelectric phase.
More Related Videos
08:21Sample Preparation in Quartz Crystal Microbalance Measurements of Protein Adsorption and Polymer Mechanics
Published on: January 22, 2020
07:02Investigating the Potential of Singly Curved Thin Piezoelectric Transducers for Energy Harvesting and Structural Health Monitoring
Published on: November 14, 2025