Elastic properties of microstructural components of human bone tissue as measured by nanoindentation

J Y Rho1, M E Roy, T Y Tsui

  • 1Department of Biomedical Engineering, University of Memphis, Memphis, Tennessee 38152, USA. jrho@cc.memphis.edu