Related Experiment Video
Updated: Aug 22, 2026

Rapid Mix Preparation of Bioinspired Nanoscale Hydroxyapatite for Biomedical Applications
Published on: February 23, 2017
Reactivity of biological and synthetic hydroxyapatite towards Zn(II) ion, solid-liquid investigations
Gigliola Lusvardi1, Ledi Menabue, Monica Saladini
1Dipartimento di Chimica, Università degli Studi di Modena e Reggio Emilia, Via G. Campi 183, 41100 Modena, Italy.
Abstract:
The reaction of biological and synthetic hydroxyapatite Ca5(PO4)3OH (HAP) with Zn2+ ions is investigated as a function of Zn2+/Ca2+ molar ratio, time, temperature and electrolyte type (NaCl, NaHCO3, Na2HPO4) by means of pH, pZn, pCa measurements, in aqueous solution. Biological powdered HAP invariably affords an almost quantitative reaction, while Zn2+ precipitated only partially by reaction with cubelets of biological HAP. Using powdered biological HAP and synthetic HAP (dried at 100 degrees C), the reaction with Zn2+ ion is fast and takes place without addition of precipitating anion; synthetic HAP (dried at 1000 degrees C) reacts if free phosphate ions are present. The solid phases separated after different reaction times are investigated by means of X-ray diffraction (XRD), IR, SEM techniques and elemental analysis (C,H,N). The solid phases contain Zn3(PO4)2.4H2O (Hopeite) at the beginning of reaction and CaZn2(PO4)2.2H2O (Scholzite) at the equilibrium.