Related Experiment Video
Updated: Jul 18, 2026

Comprehensive Characterization of Tissue Mineralization in an Ex Vivo Model
Published on: September 27, 2024
Energy absorption characterization of human enamel using nanoindentation
1Biomaterials Science Research Unit, Faculty of Dentistry, University of Sydney, NSW, Australia.
Abstract:
Enamel is a natural composite, which has much higher toughness than its major component, crystalline hydroxyapatite. In this study, the energy absorption behavior of human sound enamel was investigated with nanoindentation techniques. A UMIS nanoindenter system as well as a Berkovich and two spherical indenters with nominal tip radii of 5 and 20 microm were used to indent enamel at different loading forces in the direction parallel to enamel prisms. Inelastic energy dissipation versus depth of indenter penetration (U%-h(p) curve) as well as a function of indentation strain (U%-epsilon curve) of enamel was determined. Enamel showed much higher energy absorption capacity than a ceramic material with equivalent modulus (fused silica). Even at the lowest forces (1 mN) for the 20 microm indenter, inelastic response was found. Additional tests done at different force loading rates illustrated that load rate has little influence on P-h response of enamel. The top surface of enamel has the plastic work of indentation of approximately 5.2 nJ/microm(3). The energy absorbing ability is influenced by the very small protein rich component that exists between the hydroxyapatite nanocrystals as well as within the sheath structure surrounding the enamel rods.