Depth of cure and hardness of an indirect composite polymerized with three laboratory curing units
Naomi Tanoue1, Mahoko Murakami, Hiroyasu Koizumi
1Department of Specialized Dentistry, Nagasaki University Hospital of Medicine and Dentistry, Japan.
Abstract:
This study determined the hardness and curing depth of a light-activated indirect composite polymerized with three laboratory light-polymerizing units for the purpose of comparing the curing performance of the three units. A light-activated composite material for indirect application (Vita Zeta) was polymerized with three light-polymerizing units equipped with the following light sources: 1) one halogen lamp and two fluorescent lamps (alpha-Light II); 2) three halogen lamps (Twinkle HLG); and 3) one metal halide lamp (Twinkle LI). Knoop hardness and curing depth were determined for groups of five specimens using standardized testing methods. The results were compared using analysis of variance (ANOVA) and Scheffé's S intervals (alpha = 0.05). The Knoop hardness number (KHN) generated with the halogen-fluorescent unit (12.5 KHN) was significantly (P < 0.05) lower than those produced by the halogen unit (13.9 KHN) and the metal halide unit (14.2 KHN). Of the three units, the halogen-fluorescent unit exhibited the lowest depth of cure. Both the hardness and curing depth of the composite were influenced by the laboratory polymerizing units employed.
Related Concept Videos
Accelerated Curing of Concrete
Curing Methods
Curing of Concrete
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...