Apparatus for in situ creep testing during irradiation with high-energy neutrons from a planar neutron source
W L Barmore1, A W Ruotola, R R Vandervoort
1Lawrence Livermore Laboratory, University of California, Livermore, California 94550, USA.
Abstract:
An apparatus is described for investigating the in situ creep behavior of materials during irradiation with neutrons having a spectrum similar to that of a fusion power reactor. Techniques are discussed for remote, high-vacuum creep testing during irradiation with high-energy neutrons from a planar Be(d,n) source used on the 1.93-m Isochronous Cyclotron at the University of California at Davis. Significant effects of radiation damage on the creep of niobium at a flux of 2 x 10(16) n.m(-2) s(-1) are reported.
Related Concept Videos
Factors Affecting Creep
Further, the water/cement ratio is critical, as a lower ratio increases concrete strength, thus reducing creep. The strength of the...
Effects of Creep
Creep in Concrete