Nanoindentation methods to measure viscoelastic properties of single cells using sharp, flat, and buckling tips inside ESEM
Related Experiment Video
Updated: Jun 19, 2026

Experimental and Data Analysis Workflow for Soft Matter Nanoindentation
Published on: January 18, 2022
Mohd Ridzuan Ahmad1, Masahiro Nakajima, Seiji Kojima
1Department of Micro-Nano Systems Engineering, Nagoya University, Nagoya 464-8603, Japan. ridzuan@robo.mein.nagoya-u.ac.jp
Abstract:
In this paper, methods to measure viscoelastic properties of time-dependent materials are proposed using sharp, flat, and buckling tips inside an environmental SEM. Single W303 yeast cells were employed in this study. Each of the tips was used to indent single cells in a nanoindentation test. Three loading histories were used: 1) a ramp loading history, in which a sharp indenter was used; 2) a step loading history, in which a flat indenter was implemented; and 3) a fast unloading history, in which a buckling nanoneedle was applied. Analysis of the viscoelastic properties of single cells was performed for each of the loading histories by choosing an appropriate theory between the correspondence principle and the functional equation. Results from each of the tests show good agreement, from which strong conclusion can be drawn.
More Related Videos
08:58Atomic Force Microscopy Cantilever-Based Nanoindentation: Mechanical Property Measurements at the Nanoscale in Air and Fluid
Published on: December 2, 2022
05:49Mechano-Node-Pore Sensing: A Rapid, Label-Free Platform for Multi-Parameter Single-Cell Viscoelastic Measurements
Published on: December 2, 2022