Related Experiment Video
Updated: Jun 2, 2026

In Situ Neutron Powder Diffraction Using Custom-made Lithium-ion Batteries
Published on: November 10, 2014
In situ transmission electron microscopy observation of microstructure and phase evolution in a SnO₂ nanowire during
Chong-Min Wang1, Wu Xu, Jun Liu
1Environmental Molecular Sciences Laboratory, Pacific Northwest National Laboratory, Richland, Washington 99352, United States. Chongmin.Wang@pnl.gov
Abstract:
Recently we have reported structural transformation features of SnO(2) upon initial charging using a configuration that leads to the sequential lithiation of SnO(2) nanowire from one end to the other (Huang et al. Science2010, 330, 1515). A key question to be addressed is the lithiation behavior of the nanowire when it is fully soaked into the electrolyte (Chiang Science2010, 330, 1485). This Letter documents the structural characteristics of SnO(2) upon initial charging based on a battery assembled with a single nanowire anode, which is fully soaked (immersed) into an ionic liquid based electrolyte using in situ transmission electron microscopy. It has been observed that following the initial charging the nanowire retained a wire shape, although highly distorted. The originally straight wire is characterized by a zigzag structure following the phase transformation, indicating that during the phase transformation of SnO(2) + Li ↔ Li(x)Sn + Li(y)O, the nanowire was subjected to severe deformation, as similarly observed for the case when the SnO(2) was charged sequentially from one end to the other. Transmission electron microscopy imaging revealed that the Li(x)Sn phase possesses a spherical morphology and is embedded into the amorphous Li(y)O matrix, indicating a simultaneous partitioning and coarsening of Li(x)Sn through Sn and Li diffusion in the amorphous matrix accompanied the phase transformation. The presently observed composite configuration gives detailed information on the structural change and how this change takes place on nanometer scale.
More Related Videos
11:03Nanoscale Characterization of Liquid-Solid Interfaces by Coupling Cryo-Focused Ion Beam Milling with Scanning Electron Microscopy and Spectroscopy
Published on: July 14, 2022
10:53Preparation of Graphene Liquid Cells for the Observation of Lithium-ion Battery Material
Published on: February 5, 2019