Related Experiment Video
Updated: Apr 16, 2026

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model
Published on: May 23, 2018
Cooperation between adsorbates accounts for the activation of atomic layer deposition reactions
Mahdi Shirazi1, Simon D Elliott
1Tyndall National Institute, University College Cork, Lee Maltings, Cork, Ireland. simon.elliott@tyndall.ie.
Abstract:
Atomic layer deposition (ALD) is a technique for producing conformal layers of nanometre-scale thickness, used commercially in non-planar electronics and increasingly in other high-tech industries. ALD depends on self-limiting surface chemistry but the mechanistic reasons for this are not understood in detail. Here we demonstrate, by first-principle calculations of growth of HfO2 from Hf(N(CH3)2)4-H2O and HfCl4-H2O and growth of Al2O3 from Al(CH3)3-H2O, that, for all these precursors, co-adsorption plays an important role in ALD. By this we mean that previously-inert adsorbed fragments can become reactive once sufficient numbers of molecules adsorb in their neighbourhood during either precursor pulse. Through the calculated activation energies, this 'cooperative' mechanism is shown to have a profound influence on proton transfer and ligand desorption, which are crucial steps in the ALD cycle. Depletion of reactive species and increasing coordination cause these reactions to self-limit during one precursor pulse, but to be re-activated via the cooperative effect in the next pulse. This explains the self-limiting nature of ALD.
Related Concept Videos
Adsorption of Gases on Solids
Adsorption Isotherms II
Adsorption Isotherms I
Atomic Absorption Spectroscopy: Atomization Methods
Atomic Absorption Spectroscopy: Lab
Solutions containing organic solvents, such as low-molecular-mass alcohols, esters, or ketones, enhance absorbances by increasing...
Atomic Absorption Spectroscopy: Interference
Spectral interference occurs when signals from other elements or molecules overlap with the analyte signal, falsely elevating or masking the analyte's absorbance. This interference can be corrected using Zeeman,...