Pd nanoparticles on ZnO-passivated porous carbon by atomic layer deposition: an effective electrochemical catalyst
Xiangyi Luo1,2, Mar Piernavieja-Hermida3, Jun Lu1
1Chemical Sciences and Engineering Division, Argonne National Labaratory, Argonne, IL 60439, USA.
Abstract:
Uniformly dispersed Pd nanoparticles on ZnO-passivated porous carbon were synthesized via an atomic layer deposition (ALD) technique, which was tested as a cathode material in a rechargeable Li-O2 battery, showing a highly active catalytic effect toward the electrochemical reactions-in particular, the oxygen evolution reaction. Transmission electron microscopy (TEM) showed discrete crystalline nanoparticles decorating the surface of the ZnO-passivated porous carbon support in which the size could be controlled in the range of 3-6 nm, depending on the number of Pd ALD cycles performed. X-ray absorption spectroscopy (XAS) at the Pd K-edge revealed that the carbon-supported Pd existed in a mixed phase of metallic palladium and palladium oxide. The ZnO-passivated layer effectively blocks the defect sites on the carbon surface, minimizing the electrolyte decomposition. Our results suggest that ALD is a promising technique for tailoring the surface composition and structure of nanoporous supports for Li-O2 batteries.
Related Concept Videos
Batteries and Fuel Cells
Atomic Radii and Effective Nuclear Charge
What is an Electrochemical Gradient?
The chemical gradient relies on differences in the abundance of a substance on the outside versus the inside of a cell and flows from areas of high to low ion concentration. In contrast, the electrical gradient revolves around an...
Atomic Spectroscopy: Effects of Temperature
At thermal equilibrium, the relative populations of excited and ground state atoms can be estimated using the Maxwell–Boltzmann distribution. For example, an increase in temperature...
The Carbon Cycle
Carbon Skeletons