1Physique de la Matière Condensée, Collège de France, 11, place Marcelin-Berthelot, 75231 Paris cedex 05, France Department of Physics, Graduate School of Humanities and Sciences, Ochanomizu University, 2-1-1, Otsuka, Bunkyo-ku, 112-8610, Japan, Bunkyo-ku, France.
Abstract:
In our previous paper (Eur. Phys. J. E 4, 121 (2001)) we proposed a coarse-grained elastic energy for nacre, or stratified structure of hard and soft layers found in certain seashells . We then analyzed a crack running perpendicular to the layers and suggested one possible reason for the enhanced toughness of this substance. In the present paper, we consider a crack running parallel to the layers. We propose a new term added to the previous elastic energy, which is associated with the bending of layers. We show that there are two regimes for the parallel-fracture solution of this elastic energy; near the fracture tip the deformation field is governed by a parabolic differential equation while the field away from the tip follows the usual elliptic equation. Analytical results show that the fracture tip is lenticular, as suggested in a paper on a smectic liquid crystal (P.G. de Gennes, Europhys. Lett. 13, 709 (1990)). On the contrary, away from the tip, the stress and deformation distribution recover the usual singular behaviors ( and 1/, respectively, where x is the distance from the tip). This indicates there is no enhancement in toughness in the case of parallel fracture.
More Related Videos
05:30Crack Monitoring in Resonance Fatigue Testing of Welded Specimens Using Digital Image Correlation
Published on: September 29, 2019
07:37Full-field Strain Measurements for Microstructurally Small Fatigue Crack Propagation Using Digital Image Correlation Method
Published on: January 16, 2019
Related Concept Videos
Microcracking in Concrete
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...
Fatigue
Stress-Strain Diagram - Brittle Materials
Types of Non-structural Cracks in Concrete
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
Behavior of Concrete Under Compressive Load
As the concrete specimen fractures under...