Related Experiment Video
Updated: Mar 12, 2026

Aerosol-assisted Chemical Vapor Deposition of Metal Oxide Structures: Zinc Oxide Rods
Published on: September 14, 2017
Single-walled carbon nanotubes coated with ZnO by atomic layer deposition
Partha P Pal1,2, Evgenia Gilshteyn3, Hua Jiang1
1Department of Applied Physics, Aalto University School of Science, PO Box 15100, FI-00076, Espoo, Finland.
Abstract:
The possibility of ZnO deposition on the surface of single-walled carbon nanotubes (SWCNTs) with the help of an atomic layer deposition (ALD) technique was successfully demonstrated. The utilization of pristine SWCNTs as a support resulted in a non-uniform deposition of ZnO in the form of nanoparticles. To achieve uniform ZnO coating, the SWCNTs first needed to be functionalized by treating the samples in a controlled ozone atmosphere. The uniformly ZnO coated SWCNTs were used to fabricate UV sensing devices. An UV irradiation of the ZnO coated samples turned them from hydrophobic to hydrophilic behaviour. Furthermore, thin films of the ZnO coated SWCNTs allowed us switch p-type field effect transistors made of pristine SWCNTs to have ambipolar characteristics.
More Related Videos
12:47Preparation and Use of Photocatalytically Active Segmented Ag|ZnO and Coaxial TiO2-Ag Nanowires Made by Templated Electrodeposition
Published on: May 2, 2014
09:20Fabrication of Low Temperature Carbon Nanotube Vertical Interconnects Compatible with Semiconductor Technology