New Surface-Treatment Technique of Concrete Structures Using Crack Repair Stick with Healing Ingredients

Tae-Ho Ahn1, Hong-Gi Kim2, Jae-Suk Ryou3

  • 1International Sustainable Engineering Materials (ISEM) Center, Ceramic Materials Institute & Division of Advanced Materials Science Engineering, Hanyang University, 222 Wangsimni-ro, Seongdong-gu, Seoul 133-79, Korea. thahn@hanyang.ac.kr.

Related Concept Videos

Curing Methods01:26

Curing Methods

Concrete members with a small surface-to-volume ratio are cured by oiling and moistening the forms before casting the concrete member. These forms can be left in place for a prolonged period to prevent moisture loss, and can be wetted if made of a material suitable for wetting. If the forms are removed early, the concrete member is moistened and covered with polythene sheets to maintain moisture. For large horizontal concrete surfaces exposed to dry weather, a temporary covering is suspended...
347
Accelerated Curing of Concrete01:25

Accelerated Curing of Concrete

Accelerating concrete curing is achieved by applying heat and additional moisture. This process accelerates the hydration of the cement, resulting in an earlier strength gain in the concrete. Steam curing is a method wherein the concrete products are either transported through a chamber on a conveyor belt or encased in plastic, allowing steam at atmospheric pressure to circulate freely around them. This process begins with a phase of moist curing that typically lasts between 3 to 5 hours, after...
514
Types of Non-structural Cracks in Concrete01:28

Types of Non-structural Cracks in Concrete

Non-structural cracks are primarily of three types: plastic, early-age thermal, and drying shrinkage cracks. Plastic cracks are further classified into plastic shrinkage cracks and plastic settlement cracks.
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
541
Curing of Concrete01:20

Curing of Concrete

The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
407
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
512
Mass Concreting01:22

Mass Concreting

Mass concreting refers to the process of placing large volumes of concrete, such as in gravity dams. The heat generated during the cement hydration process and differential cooling rates within the concrete mass can lead to a temperature gradient, which can result in thermal cracks in the concrete mass.
To reduce the risk of such cracking, the concrete mix may incorporate low-heat cement and pozzolans to reduce the temperature rise. Pre-cooled angular aggregates and water-reducing admixtures...