Objective:
The aim of this study was to measure the effect of irradiation with a novel 445-nm diode laser on the shear bond strength (SBS) of ceramic brackets before debonding.
Materials And Methods:
Thirty ceramic brackets (In-Ovation® C, GAC) were bonded in standard manner to the planed and polished buccal enamel surfaces of 30 caries-free human third molars. Each tooth was randomly allocated to the laser or control group, with 15 samples per group. The brackets in the laser group were irradiated with the diode laser (SIROLaser Blue®; Sirona) on three sides of the bracket bases for 5 sec each (lateral-coronal-lateral, a total of 15 sec) immediately before debonding. SBS values were measured for the laser group and control group. To assess the adhesive remnant index (ARI) and the degree of enamel fractures, micrographs of the enamel surface were taken with 10-fold magnification after debonding.
Results:
The SBS values were significantly lower statistically in the laser group in comparison with the control group (p < 0.05). The ARI scores were also significantly lower statistically in the laser group in comparison with the control group (p < 0.05). No bracket fractures or enamel fractures occurred in either group after debonding.
Conclusions:
Irradiation of ceramic brackets with the novel diode laser before debonding significantly reduces the SBS values. This is of clinical importance, as it means that the risk of damage to the teeth, bracket fractures, and the overall treatment time can be reduced.