Initial Discharge Behavior of an Ultra High Loading 3D Sulfur Cathode for a Room-Temperature Na/S Battery
Icpyo Kim1, Changhyeon Kim1, Huihun Kim1
1Department of Materials Engineering and Convergence Technology, RIGET, Gyeongsang National University, Jinju 52828, Republic of Korea.
Abstract:
A 3D sulfur cathode for a large-scale room-temperature (RT) Na/S battery with a high sulfur loading of 14.63 mg cm-2 was fabricated. The first discharge was tested in order to understand the macroscopic changes. A first discharge capacity of 865 mAh g-1 was obtained at 1/1000 C-rate along with a discharge curve with two clear plateaus at 2.29 V and 1.78 V, respectively. A visual change occurs in the 3D sulfur cathode. A thick layer of discharge products at the solid electrolyte separator face of the 3D sulfur cathode was observed and analyzed using a scanning electron microscope (SEM) coupled with energy dispersive X-ray spectroscopy (EDS).
More Related Videos
10:03Characterization of Electrode Materials for Lithium Ion and Sodium Ion Batteries Using Synchrotron Radiation Techniques
Published on: November 11, 2013
11:04Synthesis of Ionic Liquid Based Electrolytes, Assembly of Li-ion Batteries, and Measurements of Performance at High Temperature
Published on: December 20, 2016
Related Concept Videos
Batteries and Fuel Cells
The Sulfur Cycle
Behavior of Concrete Under Compressive Load
As the concrete specimen fractures under...
Sulfur Assimilation
Discharge Summary Forms
Here's a detailed look at the key components and guidelines for preparing a discharge summary:
Initiation of Translation
First, the initiator tRNA must be selected from the pool of elongator tRNAs by eukaryotic initiation factor 2 (eIF2). The initiator tRNA (Met-tRNAi) has conserved sequence elements including modified bases at...