Does radiopaque cement conceal periprosthetic bone loss around femoral stems?
Bernhard Flatøy1,2, Jon Dahl1, Stephan Maximilian Röhrl1
1Division of Orthopaedic Surgery, Oslo University Hospital, Oslo, Norway.
Background:
Periprosthetic bone remodelling may increase fracture risk and deplete bone stock around hip implants. These changes are in part caused by implant design, advocating an early evaluation of bone remodelling properties of new implants. This can be done by repeated dual-energy x-ray absorptiometry (DXA) measurements. We know that radiopaque cement falsely elevates bone mineral density (BMD) in single measurements, however, its impact on repeated measurements, i.e. BMD changes is unexplored. We have therefore investigated whether the presence of radiopaque cement affect repeated BMD measurements.
Methods:
33 patients eligible for total hip replacement were randomly assigned to either radiopaque or radiolucent cement. BMD changes up to 12 months were measured by DXA, in addition to Harris Hip Score, plain radiographs and radiostereometric analysis (RSA).
Results:
Periprosthetic BMD declined during the first 3-6 months in all zones in both groups. The greatest reduction (14%) was seen in the proximal Gruen zones (1 and 7). We found a significant difference in Gruen zones 1 and 2, where the measured bone loss was higher in the radiolucent cement group.
Conclusions:
The presence of radiopaque agents in bone cement may influence DXA measurements of bone remodelling.ClinicalTrials.gov identifier NCT00473421.
Related Concept Videos
Hydration of Cement
Soundness of Cement
Line Loss
Line loss impacts power delivery efficiency in a balanced three-phase circuit. The symmetry in such a circuit simplifies the...
Portland Cement
Fineness of Cement
Direct...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...