Mechanical Properties of Ultra-High Performance Concrete before and after Exposure to High Temperatures
How-Ji Chen1, Yi-Lin Yu1, Chao-Wei Tang2,3,4
1Department of Civil Engineering, National Chung-Hsing University, No. 250, Kuo Kuang Road, Taichung 402, Taiwan.
Abstract:
Compared with ordinary concrete, ultra-high performance concrete (UHPC) has excellent toughness and better impact resistance. Under high temperatures, the microstructure and mechanical properties of UHPC may seriously deteriorate. As such, we first explored the properties of UHPC with a designed 28-day compressive strength of 120 MPa or higher in the fresh mix phase, and measured its hardened mechanical properties at seven days. The test variables included: the type of cementing material and the mixing ratio (silica ash, ultra-fine silicon powder), the type of fiber (steel fiber, polypropylene fiber), and the fiber content (volume percentage). In addition to the UHPC of the experimental group, pure concrete was used as the control group in the experiment; no fiber or supplementary cementitious materials (silica ash, ultra-fine silicon powder) were added to enable comparison and discussion and analysis. Then, the UHPC-1 specimens of the experimental group were selected for further compressive, flexural, and splitting strength tests and SEM observations after exposure to different target temperatures in an electric furnace. The test results show that at room temperature, the 56-day compressive strength of the UHPC-1 mix was 155.8 MPa, which is higher than the >150 MPa general compressive strength requirement for ultra-high-performance concrete. The residual compressive strength, flexural strength, and splitting strength of the UHPC-1 specimen after exposure to 300, 400, and 500 °C did not decrease significantly, and even increased due to the drying effect of heating. However, when the temperature was 600 °C, spalling occurred, so the residual mechanical strength rapidly declined. SEM observations confirmed that polypropylene fibers melted at high temperatures, thereby forming other channels that helped to reduce the internal vapor pressure of the UHPC and maintain a certain residual strength.
More Related Videos
10:52Conducting Elevated Temperature Normal and Combined Pressure-Shear Plate Impact Experiments Via a Breech-end Sabot Heater System
Published on: August 7, 2018
07:15A Testing Platform for Durability Studies of Polymers and Fiber-reinforced Polymer Composites under Concurrent Hygrothermo-mechanical Stimuli
Published on: December 11, 2014
Related Concept Videos
Hot Weather Concreting
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Cold Weather Concreting
To counteract the negative impacts of cold weather, ensuring...
Mass Concreting
To reduce the risk of such cracking, the concrete mix may incorporate low-heat cement and pozzolans to reduce the temperature rise. Pre-cooled angular aggregates and water-reducing admixtures...
Frost Resistant Concrete
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...