Hydrotalcite stability during long-term exposure to natural environmental conditions

Virginia Alonso-de-Linaje1,2, Dominique J Tobler3, Rubén Espinosa4,5

  • 1AECOM Environment, c/Alfonso XII, 62, 28014, Madrid, Spain. v.alonsodelinaje@usal.com.

Related Concept Videos

Hydration of Cement01:24

Hydration of Cement

Hydration of cement is a chemical reaction between cement particles and water. This process occurs primarily through two mechanisms: through-solution and topochemical. In the through-solution process, anhydrous compounds dissolve into their constituents, hydrates form in the solution, and then precipitate from the supersaturated solution. The topochemical process involves solid-state reactions at the cement particle surface. The through-solution process dominates the topochemical process at the...
670
Strength and Heat of Hydration01:29

Strength and Heat of Hydration

The hydration of cement is an exothermic reaction in which heat is generated as cement hydrates. This heat of hydration is critical to cement's strength development. The rate at which this heat is generated affects the temperature rise, with a majority of the heat being released early in the hydration process, half within the first three days, and about 75% within the first week.
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
563
Sulfate Attack on Concrete01:29

Sulfate Attack on Concrete

Sulfate attack on concrete is a deterioration process characterized by a whitish discoloration beginning at the edges and corners, accompanied by cracking and spalling. This phenomenon occurs when sulfates react with the components of hardened concrete, forming compounds like calcium sulfate and calcium sulfoaluminate which occupy more space than the substances they replace, causing the concrete to expand and disrupt.
Sulfates from sources like soil, groundwater, or industrial effluents...
600
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
316
Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...
408
Carbonation Shrinkage01:24

Carbonation Shrinkage

Atmospheric CO2 penetrates the concrete's pores and, in the presence of moisture, forms carbonic acid, which then reacts with calcium hydroxide in the hydrated cement, forming calcium carbonate. This process reduces the concrete's volume and is termed carbonation shrinkage.
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction...