A shear test for the bond strength of ceramometals
I A Hammad1, R J Goodkind, W W Gerberich
1Division of Graduate Prosthodontics, University of Minnesota, School of Dentistry, Minneapolis.
Abstract:
An innovative shear-testing method was introduced to study the effect of firing temperature, type of metal, and surface texture on the bond strength of the ceramometals. Two common ceramic/metal alloys were used: Olympia, a precious alloy, and Talladium, a base alloy. A Ceramco II Paint-O-Pake opaque was selected for the study. Each porcelain alloy was prepared in a similar manner before porcelain application to achieve uniform surfaces. A separate category of base alloy samples was subjected to etching after sandblasting. Each category was then divided into two groups. Opaque porcelain was fired according to the manufacturer's instructions in one group and 65 degrees F higher in the other. The bond strengths were compared by statistical analysis and post-tested samples were evaluated visually and microscopically with a scanning electron microscope.
Related Concept Videos
Bonding in Metals
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as the...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Bonding and Strength of Aggregate
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...