Fractographic characterization of isotactic polypropylene fibers
Taha Z N Sokkar1, Mohammed A El-Bakary1, Amira A S Azzam1
1Physics Department, Faculty of Science, Mansoura University, Mansoura, Egypt.
Abstract:
In this article we present an opto-thermo-mechanical characterization of isotactic polypropylene monofilament during failure by fracture. The digital photoelasticity, the two-beam Pluta polarising interference microscope and the computed tomography are used to provide quantitative data and visual models of the fracture regions of isotactic polypropylene fibers suffering failure by fracture at different thermal and mechanical conditions. Birefringence values and the intrinsic stress-anisotropy are measured at the fracture surface. 3D models of the fracture regions are reconstructed. Photoelastic patterns and two-beam interferograms are included for illustration.
Related Concept Videos
Polymer Classification: Stereospecificity
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Polymer Classification: Architecture
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...
Characteristics and Nomenclature of Copolymers