Silica and Silica-Titania Xerogels Doped with Iron(III) for Total Antioxidant Capacity Determination
Maria A Morosanova1, Ksenia V Chaikun2, Elena I Morosanova1
1Analytical Chemistry Division, Chemistry Department, Lomonosov Moscow State University, 119234 Moscow, Russia.
Abstract:
In order to design a sensor material for total antioxidant capacity determination we have prepared silica and silica-titania xerogels doped with iron(III) and modified with 1,10-phenanthroline. Titanium(IV) tetraethoxyde content in the precursors (titanium(IV) tetraethoxyde and tetraethyl orthosilicate) mixtures has been varied from 0 to 12.5% vol. Iron(III) concentrations in sol has been varied from 1 to 100 mM. The increase of titanium(IV) content has led to a decrease in BET surface area and average pore diameter and an increase of micropore surface area and volume, which has resulted in better iron(III) retention in the xerogels. Iron(III), immobilized in the xerogel matrix, retains its ability to form complexes with 1,10-phenanthroline and to be reduced to iron(II). Static capacities for 1,10-phenanthroline have been determined for all the iron(III) doped xerogels (0.207 mmol/g-0.239 mmol/g) and they are not dependent on the iron(III) content. Sensor materials-xerogels doped with iron(III) and modified with 1,10-phenanthroline-have been used for antioxidants (catechol, gallic and ascorbic acids, and sulphite) solid phase spectrophotometric determination. Limits of detection for catechol, gallic and ascorbic acids, and sulphite equal 7.8 × 10-6 M, 5.4 × 10-6 M, 1.2 × 10-5 M, and 3.1 × 10-4 M, respectively. The increase of titanium(IV) content in sensor material has led to an increase of the reaction rate and the sensitivity of determination. Proposed sensor materials have been applied for total antioxidant capacity (in gallic acid equivalents) determination in soft beverages, have demonstrated high stability, and can be stored up to 6 months at room temperature.
More Related Videos
11:47The Effect of Interfacial Chemical Bonding in TiO2-SiO2 Composites on Their Photocatalytic NOx Abatement Performance
Published on: July 4, 2017
10:30A Generalized Method for Determining Free Soluble Phenolic Acid Composition and Antioxidant Capacity of Cereals and Legumes
Published on: June 10, 2022