Experimental Study of Mechanical Properties of Polypropylene Random Copolymer and Rice-Husk-Based Biocomposite by
Fahad Ali Rabbani1, Saima Yasin2, Tanveer Iqbal1
1Department of Chemical, Polymer & Composite Materials Engineering, University of Engineering and Technology, Lahore (New Campus), Kala Shah Kaku 39020, Pakistan.
Abstract:
Nanoindentation is widely used to investigate the surface-mechanical properties of biocomposites. In this study, polypropylene random copolymer (PPRC) and biowaste rice husk (BRH) were used as the main raw materials, and glass-fiber-reinforced polypropylene and talc were also used with BRH to enhance the mechanical characterization of the biocomposites. The interfacial bonding between the polymer and the rice husk was increased by treating them with maleic anhydride and NaOH, respectively. The results obtained from the nanoindentation indicated that the plastic behavior of the biocomposites was prominent when untreated BRH was used and vice versa. The modulus and hardness of the biocomposite improved by 44.8% and 54.8% due to the neat PPRC, respectively. The tribological properties were studied based on the hardness-to-modulus ratio and it was found that BRH- and talc-based biocomposites were better than other samples in terms of low friction and wear rate. The creep measurements showed that untreated rice husk biocomposite exhibited high resistance to load deformation.
More Related Videos
09:06The Effect of Construction and Demolition Waste Plastic Fractions on Wood-Polymer Composite Properties
Published on: June 7, 2020
08:58Atomic Force Microscopy Cantilever-Based Nanoindentation: Mechanical Property Measurements at the Nanoscale in Air and Fluid
Published on: December 2, 2022
Related Concept Videos
Classification and Mechanical Properties of Synthetic Polymers
Bioplastics