Effect of Backbone Rigidity on the Glass Transition of Polymers of Intrinsic Microporosity Probed by Fast Scanning

Huajie Yin1, Bin Yang2, Yeong Zen Chua2

  • 1Bundesanstalt für Materialforschung und -prüfung (BAM), Unter den Eichen 87, 12205 Berlin, Germany.

ACS Macro Letters
|May 27, 2022
PubMed

Related Concept Videos

Polymer Classification: Crystallinity01:21

Polymer Classification: Crystallinity

Unlike ionic or small covalent molecules, polymers do not form crystalline solids due to the diffusion limitations of their long-chain structures. However, polymers contain microscopic crystalline domains separated by amorphous domains.
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
3.2K
Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
275
Polymers: Molecular Weight Distribution01:10

Polymers: Molecular Weight Distribution

For any given polymer, the weight average molecular weight (Mw) is higher than, if not equal to, the number average molecular weight (Mn). The only situation in which the weight average molecular weight and the number average molecular weight are equal is when a polymer consists only of chains with equal molecular weight. However, this never happens in a synthetic polymer, since it is difficult to control the polymerization process up to a molecular level with accuracy to a hundred percent.
3.8K
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity01:15

Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity

Deformation occurs in axial and transverse directions when an axial load is applied to a slender bar. This deformation impacts the cubic element within the bar, transforming it into either a rectangular parallelepiped or a rhombus, contingent on its orientation. This transformation process induces shearing strain. Axial loading elicits both shearing and normal strains. Applying an axial load instigates equal normal and shearing stresses on elements oriented at a 45° angle to the load axis.
339
¹H NMR of Conformationally Flexible Molecules: Variable-Temperature NMR01:15

¹H NMR of Conformationally Flexible Molecules: Variable-Temperature NMR

The axial and equatorial protons in cyclohexane can be distinguished by performing a variable-temperature NMR experiment. In this process, except for one proton, the remaining eleven protons are replaced by deuterium. The deuterium substitution avoids the possible peak splitting caused by the spin-spin coupling between the adjacent protons. The remaining proton flips between the axial and equatorial positions.
1.2K
Molecular Weight of Step-Growth Polymers01:08

Molecular Weight of Step-Growth Polymers

Step growth polymerization involves bi or multifunctional monomers. Bifunctional monomers react to form linear step growth polymers, whereas multifunctional monomers react to form non-linear or branched polymers.
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
2.3K