Related Experiment Video
Updated: Aug 16, 2025

Experimental Protocol to Investigate Particle Aerosolization of a Product Under Abrasion and Under Environmental Weathering
Published on: September 16, 2016
Effect of Spraying Polyurea on the Anti-Blast Performance of the Ultra-High Performance Concrete Slab
Bin Gao1, Jun Wu1, Qinyi Chen1
1School of Urban Rail Transportation, Shanghai University of Engineering Science, Shanghai 201620, China.
Abstract:
Recently, polyurea has been applied to improve the anti-blast performance of metal plates, masonry walls, and concrete structures. However, the strengthening effectiveness of polyurea on ultra-high performance concrete (UHPC) slabs with an overall response is still unclear. Hence, this paper examined the strengthening effectiveness of polyurea on the anti-blast performance of UHPC slabs under near-field explosion by the finite element (FE) method. First, a benchmark finite element model for UHPC and polyurea-UHPC (PUHPC) slabs under blast loading was established and validated by field blast tests, with scaled distances ranging from 0.4 m/kg1/3 to 0.8 m/kg1/3. After that, parametric analysis was conducted to fully understand the strengthening effectiveness of polyurea on the anti-blast performance of the UHPC slab. Factors including the scaled distance, polyurea thickness, span-to-depth ratio of the slab, and longitudinal reinforcement ratio were considered. The results showed that (1) spraying polyurea on the rear face of the UHPC slab can reduce the width of cracks and mitigate the damage of specimens; (2) the strengthening effectiveness of polyurea on the UHPC slab became prominent when the UHPC slab suffered a larger maximum deflection; (3) in terms of the deflection and energy absorption capacity of PUHPC slabs, the optimum thickness of sprayed polyurea was determined to be 8 mm to 12 mm; and (4) by adopting the multiple nonlinear regression method, a prediction formula was developed to quickly obtain the end rotation of the UHPC slab strengthened with polyurea under near-field explosions.
Related Concept Videos
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Effects of Air-entrainment in Concrete
Superplasticizers
Frost Resistant Concrete
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
Shotcrete
Accelerated Curing of Concrete