Effect of different chelating agents on the shear bond strength of calcium silicate-based cements to coronal dentin
Mohamed Ahmed Elsayed1,2, Md Sofiqul Islam3, Karim Elbeltagy4
1Department of Endodontics, RAK College of Dental Sciences, RAK Medical and Health Sciences University, United Arab Emirates.
Abstract:
We evaluated the shear bond strength (SBS) of mineral trioxide aggregate (MTA) and Biodentine (BD) to coronal dentin after treatment with ethylenediaminetetraacetic acid (EDTA), phytic acid (IP6), or etidronic acid (HEDP). Sodium hypochlorite-treated dentin surfaces were randomly divided into four groups according to conditioning protocol namely, 17% EDTA, 2.5% IP6, 9% HEDP, or distilled water (DS). Specimens were further divided according to the type of cement placed on conditioned dentin and SBS was tested. The results showed that DS/MTA and IP6/MTA groups had the highest values, and there was no significant difference between these two groups. IP6/BD group showed a lower SBS value compared to IP6/MTA; however, this did not reach the level of significance. The BS to dentin was influenced by the type of calcium silicate material and chelating agent. IP6 either improved or maintained the bonding while EDTA and HEDP showed a negative or no influence effect.
More Related Videos
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
08:26Development of Amelogenin-chitosan Hydrogel for In Vitro Enamel Regrowth with a Dense Interface
Published on: July 10, 2014
Related Concept Videos
Bonding and Strength of Aggregate
Hydration of Cement
Complexation Equilibria: The Chelate Effect
Masking and Demasking Agents
There are many masking agents, such as cyanide, fluoride, triethanolamine, thiourea, and 2,3-bis(sulfanyl)propan-1-ol (formerly 2,3-dimercapto-1-propanol), with the masking agent chosen based on...
Ionic Strength: Effects on Chemical Equilibria
In this solution, the primary...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...