Related Experiment Video
Updated: Jul 27, 2025

Roughness Impact of Piezoelectric Dental Scaler on Two Distinct Flowable Composite Filling Materials
Published on: January 10, 2025
12-Month flexural mechanical properties of conventional and self-adhesive flowable resin composite materials
John Brewster1, Howard W Roberts2
155th DS/SGDR.
Abstract:
The aim of this study was to investigate the 12-month flexural mechanical properties of 23 flowable resin-based composites (FRBC) that included 5 self-adhesive FRBC materials. Specimens were evaluated following ISO 4049:2019 guidelines, but additionally stored in physiologic 0.2M phosphate buffered saline solution being tested at 24 h, 1 week, 1 month, and at 3-, 6-, 9-, and 12-months. While some deviation and degradation were noted at testing intervals, conventional FRBC materials overall demonstrated greater flexural strength than the self-adhesive and compomer materials. Three self-adhesive materials and the compomer were below recommended ISO 4049:2019 flexural strength values at 24 h with another after 6 months storage. Conventional FRBC materials, except at 1 month, overall demonstrated increased flexural modulus than the self-adhesive FRBC materials. Although results were material dependent, conventional FRBC materials demonstrated overall greater flexural mechanical properties as compared to the self-adhesive FRBC materials and the compomer evaluated.
More Related Videos
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
09:54Author Spotlight: Enhancing Fiber Composite Laminate Quality with the Wet Hand Lay-Up/Vacuum Bag Process
Published on: June 30, 2023
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to...
Flow Table Test
Concrete is placed within a truncated cone mold that is 8 inches high with an 8-inch base diameter and a 5-inch top diameter. The...