Role of a cyclopentadienyl ligand in a heteroleptic alkoxide precursor in atomic layer deposition

Hwi Yoon1, Yujin Lee1,2, Ga Yeon Lee3

  • 1School of Electrical and Electronic Engineering, Yonsei University, 50 Yonsei-Ro, Seodaemun-Gu, Seoul 03722, South Korea.

PubMed

Related Concept Videos

[4+2] Cycloaddition of Conjugated Dienes: Diels–Alder Reaction01:16

[4+2] Cycloaddition of Conjugated Dienes: Diels–Alder Reaction

The Diels–Alder reaction is an example of a thermal pericyclic reaction between a conjugated diene and an alkene or alkyne, commonly referred to as a dienophile. The reaction involves a concerted movement of six π electrons, four from the diene and two from the dienophile, forming an unsaturated six-membered ring. As a result, these reactions are classified as [4+2] cycloadditions.
10.2K
Cycloaddition Reactions: MO Requirements for Thermal Activation01:16

Cycloaddition Reactions: MO Requirements for Thermal Activation

Thermal cycloadditions are reactions where the source of activation energy needed to initiate the reaction is provided in the form of heat. A typical example of a thermally-allowed cycloaddition is the Diels–Alder reaction, which is a [4 + 2] cycloaddition. In contrast, a [2 + 2] cycloaddition is thermally forbidden.
3.6K
Diels–Alder Reaction Forming Cyclic Products: Stereochemistry01:28

Diels–Alder Reaction Forming Cyclic Products: Stereochemistry

The Diels–Alder reaction is one of the robust methods for synthesizing unsaturated six-membered rings. The reaction involves a concerted cyclic movement of six π electrons: four π electrons from the diene and two π electrons from the dienophile.
3.9K
Preparation of Epoxides03:00

Preparation of Epoxides

Overview
Epoxides result from alkene oxidation, which can be achieved by a) air, b) peroxy acids, c) hypochlorous acids, and d) halohydrin cyclization.
Epoxidation with Peroxy Acids
Epoxidation of alkenes via oxidation with peroxy acids involves the conversion of a carbon–carbon double bond to an epoxide using the oxidizing agent meta-chloroperoxybenzoic acid, commonly known as MCPBA. Since the O–O bond of peroxy acids is very weak, the addition of electrophilic oxygen of...
7.7K
Cycloaddition Reactions: MO Requirements for Photochemical Activation01:12

Cycloaddition Reactions: MO Requirements for Photochemical Activation

Some cycloaddition reactions are activated by heat, while others are initiated by light. For example, a [2 + 2] cycloaddition between two ethylene molecules occurs only in the presence of light. It is photochemically allowed but thermally forbidden.
2.1K
Cycloaddition Reactions: Overview01:16

Cycloaddition Reactions: Overview

Cycloadditions are one of the most valuable and effective synthesis routes to form cyclic compounds. These are concerted pericyclic reactions between two unsaturated compounds resulting in a cyclic product with two new σ bonds formed at the expense of π bonds. The [4 + 2] cycloaddition, known as the Diels–Alder reaction, is the most common. The other example is a [2 + 2] cycloaddition.
2.6K