Jove
Visualize
Contact Us
JoVE
x logofacebook logolinkedin logoyoutube logo
ABOUT JoVE
OverviewLeadershipBlogJoVE Help Center
AUTHORS
Publishing ProcessEditorial BoardScope & PoliciesPeer ReviewFAQSubmit
LIBRARIANS
TestimonialsSubscriptionsAccessResourcesLibrary Advisory BoardFAQ
RESEARCH
JoVE JournalMethods CollectionsJoVE Encyclopedia of ExperimentsArchive
EDUCATION
JoVE CoreJoVE BusinessJoVE Science EducationJoVE Lab ManualFaculty Resource CenterFaculty Site
Terms & Conditions of Use
Privacy Policy
Policies

Related Concept Videos

Atomic Absorption Spectroscopy: Instrumentation01:22

Atomic Absorption Spectroscopy: Instrumentation

2.1K
An atomic absorption spectrophotometer (AAS) comprises several components: a radiation source, an atomizer, a monochromator, and a detector. The radiation source can be a hollow-cathode lamp (HCL) or an electrodeless-discharge lamp (EDL), both of which provide a narrow emission line of the required wavelength. However, some instruments use continuum sources and high-resolution monochromators to achieve a narrow range of radiation.
The atomizer used in AAS can be either a flame atomizer or an...
2.1K

You might also read

Related Articles

Articles linked to this work by shared authors, journal, and citation graph.

Sort by
Same author

Interaction of Molecular Hydrogen on α-Pu at 300 K: Nucleation of Hydrides and Pu-Catalyzed Carbides.

Journal of the American Chemical Society·2026
Same author

Charge transfer in fcc plutonium-gallium alloys.

Journal of physics. Condensed matter : an Institute of Physics journal·2025
Same author

Chemical Solution Deposition of Protective Er<sub>2</sub>O<sub>3</sub> and Y<sub>2</sub>O<sub>3</sub> Coatings onto Stainless Steel for Molten Metal Casting using Metal-Nitrate Precursors.

ACS applied materials & interfaces·2023
Same author

Growth and passivation of individual carbon nanoparticles by C2H2 addition at high temperatures: Dependence of growth rate and evolution on material and size.

The Journal of chemical physics·2023
Same author

High-Temperature Oxidation of Single Carbon Nanoparticles: Dependence on the Surface Structure and Probing Real-Time Structural Evolution via Kinetics.

Journal of the American Chemical Society·2022
Same author

Sublimation Kinetics for Individual Graphite and Graphene Nanoparticles (NPs): NP-to-NP Variations and Evolving Structure-Kinetics and Structure-Emissivity Relationships.

Journal of the American Chemical Society·2020
Same journal

Erratum: "Highly versatile, two-color setup for high-order harmonic generation using spatial light modulators" [Rev. Sci. Instrum. 95, 073002 (2024)].

The Review of scientific instruments·2026
Same journal

Thermal correction method for accurate performance evaluation of micro-thermoelectric coolers.

The Review of scientific instruments·2026
Same journal

Correcting the energy-dependent asymmetry in low-energy muon spin rotation.

The Review of scientific instruments·2026
Same journal

Fiber-integrated acousto-optic-modulator-based phase-controlled Rydberg atomic electrometer.

The Review of scientific instruments·2026
Same journal

A top-loading point-contact spectroscopy probe with in-situ sample exchange for dilution refrigerators.

The Review of scientific instruments·2026
Same journal

Investigation of plasma characteristics in a developed large-diameter, low-aspect ratio, radio frequency plasma source with a flat spiral antenna.

The Review of scientific instruments·2026
See all related articles

Related Experiment Video

Updated: May 6, 2026

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films
08:49

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films

Published on: December 4, 2014

14.2K

An automatic multi-precursor flow-type atomic layer deposition system.

Daniel J Rodriguez1, Mai A Her2, Igor O Usov1

  • 1Engineered Materials Group (MST-7), Los Alamos National Laboratory, P.O. Box 1663, Los Alamos, New Mexico 87545, USA.

The Review of Scientific Instruments
|November 18, 2024
PubMed
Summary
This summary is machine-generated.

Two automated atomic layer deposition (ALD) reactors were developed for coating additively manufactured metal parts. The systems successfully deposited alumina films on stainless steel, demonstrating precise atomic layer control for advanced material applications.

More Related Videos

Atomically Traceable Nanostructure Fabrication
12:35

Atomically Traceable Nanostructure Fabrication

Published on: July 17, 2015

8.7K
Multi-step Variable Height Photolithography for Valved Multilayer Microfluidic Devices
10:18

Multi-step Variable Height Photolithography for Valved Multilayer Microfluidic Devices

Published on: January 27, 2017

14.3K

Related Experiment Videos

Last Updated: May 6, 2026

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films
08:49

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films

Published on: December 4, 2014

14.2K
Atomically Traceable Nanostructure Fabrication
12:35

Atomically Traceable Nanostructure Fabrication

Published on: July 17, 2015

8.7K
Multi-step Variable Height Photolithography for Valved Multilayer Microfluidic Devices
10:18

Multi-step Variable Height Photolithography for Valved Multilayer Microfluidic Devices

Published on: January 27, 2017

14.3K

Area of Science:

  • Materials Science
  • Chemical Engineering
  • Nanotechnology

Background:

  • Additively manufactured (AM) metal parts require advanced surface coatings for enhanced properties.
  • Atomic Layer Deposition (ALD) offers precise control over thin film deposition, crucial for complex geometries.

Purpose of the Study:

  • To design and present two automated ALD flow reactors for coating AM metal prints.
  • To demonstrate the capability of these reactors for uniform thin film deposition.

Main Methods:

  • Development of two distinct ALD reactor designs: one for batch processing and one for single part experiments.
  • Utilized custom LabVIEW software for automated control and in situ monitoring of temperature, pressure, and film thickness via quartz crystal microbalance.
  • Deposited alumina (Al2O3) films on AM 316L stainless steel using trimethylaluminum (TMA) and water (H2O) precursors with nitrogen (N2) purge gas.

Main Results:

  • Achieved a film thickness of approximately 55 nm after 150 ALD cycles of Al2O3.
  • Verified atomic layer-level deposition accuracy using Rutherford backscattering spectroscopy.
  • Demonstrated consistent and conformal coating on additively manufactured stainless steel substrates.

Conclusions:

  • The developed automated ALD reactors are capable of precise thin film deposition on AM metal parts.
  • The systems enable reliable, in situ monitored coating processes with atomic layer control.
  • These reactors provide a valuable tool for enhancing the surface properties of additively manufactured components.