Related Experiment Video
Updated: May 31, 2025

Advanced Self-Healing Asphalt Reinforced by Graphene Structures: An Atomistic Insight
Published on: May 31, 2022
Research on the Aging Characteristics of Simulated Asphalt Within Pavement Structures in Natural Environments
Xiang Ma1,2, Weiyi Diao1,2, Jiachen Xu1,2
1College of Civil Engineering, Nanjing Forestry University, Nanjing 210037, China.
Abstract:
The global asphalt production growth rate exceeded 10% in the past decade, and over 90% of the world's road surfaces are generated from asphalt materials. Therefore, the issue of asphalt aging has been widely researched. In this study, the aging of asphalt thin films under various natural conditions was studied to prevent the distortion of indoor simulated aging and to prevent the extraction of asphalt samples from road surfaces from impacting the aged asphalt. The aging of styrene-butadiene-styrene (SBS)-modified asphalt was simulated at four different locations on an asphalt road surface. The aging characteristics of asphalt binders across various structural layers were revealed using Fourier transform infrared spectroscopy (FTIR), atomic force microscopy (AFM), and linear amplitude scanning (LAS). The results indicate that the aging behavior of the asphalt functional group on the road surface differs from other conditions; the asphalt fatigue life of 4 months equates to the 16-month aging life of asphalt within the dense-graded asphalt road surface. After 8 months of aging, the surface smoothness of the asphalt was significantly compromised. Inside of the porous pavement, the asphalt functional group is more likely to interact with water molecules than inside the dense pavement with cracks, and the variations in roughness and the reduction in fatigue life are also more significant.
Related Concept Videos
Masonry Paving
Unsoundness of Aggregate due to Volume Change
Toughness and Hardness of Aggregate
Porosity and Absorption of Aggregate
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Design Example: Joints in Concrete Pavements
Contraction joints are typically formed by sawing a groove into the concrete shortly after it has hardened. This creates a weakened vertical plane, deliberately encouraging cracking at...