Durability of NiFe-based oxygen evolution electrocatalysts in AEM water electrolyzer under fluctuating power supply
Zhihang Wan1, Dongxue Rui1, Lanlan Wu1
1Hebei Provincial Key Laboratory of Green Chemical Technology and High Efficient Energy Saving, School of Chemical Engineering and Technology, Hebei University of Technology, Tianjin 300130, China.
Abstract:
NiFe-based materials are widely utilized as anode electrocatalysts for the oxygen evolution reaction (OER) in anion exchange membrane water electrolyzers (AEMWE). However, their performance under actual fluctuating power supply remains poorly understood. In this study, the OER performance and degradation mechanisms of various NiFe-based OER catalysts are investigated in AEMWE under both constant and fluctuating voltage conditions. Among the tested materials, NixFe1-xS exhibits the best durability under both constant and fluctuating voltages, outperforming NixFe1-xP and NiFe LDH. Notably, its stability is found to be positively correlated with the interval of voltage fluctuation. The degradation of NixFe1-xS can be attributed to a combination of irreversible and reversible losses. Accelerated durability testing reveals that irreversible loss is primarily caused by the severe collapse, dissolution and agglomeration of catalyst particles on the electrode surface under fluctuating power supply. On the other hand, the reversible loss is linked to hindered contact between the electrolyte and the electrode surface, caused by gas retention within the catalyst's porous structure. This reversible loss can be mitigated by introducing a rest period, which allows for the recovery of catalyst's performance. This work provides valuable insights into the degradation mechanisms of NiFe-based OER catalysts under fluctuating power supply in AEMWE.
Related Concept Videos
Electrolysis
Batteries and Fuel Cells
The Nernst Equation
The interconnection between standard cell potentials and various thermodynamic parameters such as the standard free energy change ΔG° and equilibrium constant K has been previously explored. For example, a redox reaction involving zinc(II) and tin(II) ions at 1 M concentration with Eºcell = +0.291 V and ΔG° = −56.2 kJ is spontaneous.