The Influence of Material and Process Parameters on Pressure Agglomeration and Properties of Pellets Produced from
Arkadiusz Gendek1, Monika Aniszewska1, Paweł Tylek2
1Department of Biosystems Engineering, Institute of Mechanical Engineering, Warsaw University of Life Sciences, Nowoursynowska 164, 02-787 Warsaw, Poland.
Abstract:
Pellets produced from raw or torrefied shredded logging residues have been investigated in the study. The research material came from pine and spruce stands in Poland, Slovakia, Czechia and Hungary. Torrefaction temperatures (Tt) of 250, 300, and 400 °C were applied. Before pressure agglomeration, 3% wheat flour was added to the torrefaction material as a binding agent. Pellets with a diameter of 8 mm were produced at constant humidity, compaction pressure (P) of 140 or 180 MPa and agglomeration temperature (Ta) of 100, 120 or 140 °C. The produced pellets were assessed for their physicomechanical parameters (density, radial compressive strength, compression ratio, modulus of elasticity), chemical parameters (extractive compounds, cellulose, lignin) and energy parameters (ash content, elemental composition, calorific value). The results were subjected to basic statistical analysis and multi-way ANOVA. The produced pellets varied in physical, mechanical, chemical and energy properties. A significant effect of torrefaction temperature, agglomeration temperature and compaction pressure on the results was observed. In terms of physicomechanical parameters, the best pellets were produced from the raw material, while in terms of energy parameters, those produced from the torrefied material were superior. Pellets of satisfactory quality produced from torrefied logging residues could be obtained at Tt = 250 °C, Ta = 120 °C and P = 180 MPa. Pellets with specific density of approximately 1.1 g·cm-3, radial compressive strength of 3-3.5 MPa, modulus of elasticity of 60-80 MPa and calorific value of 20.3-23.8 MJ·kg-1 were produced in the process.
More Related Videos
07:06Wicking Tests for Unidirectional Fabrics: Measurements of Capillary Parameters to Evaluate Capillary Pressure in Liquid Composite Molding Processes
Published on: January 27, 2017
09:05Supercritical Nitrogen Processing for the Purification of Reactive Porous Materials
Published on: May 15, 2015
Related Concept Videos
Residuals and Least-Squares Property
If the observed data point lies above the line, the residual is positive, and the line underestimates the actual data value for y. If the observed data point lies below the line, the residual is negative, and the line overestimates the actual data value for y.
The process of fitting the best-fit...
Factors Influencing Drug Absorption: Pharmaceutical Parameters
Factors Influencing Drug Absorption: Anatomical Parameters
Factors Influencing Drug Absorption: Physicochemical Parameters
Enhanced drug absorption can be achieved by reducing particle sizes and increasing surface areas, thereby facilitating...
Pressure and Volume in an Adiabatic Process
The Mantel-Cox Log-Rank Test