Related Experiment Video
Updated: Jul 4, 2026

Shrinkage of Dental Composite in Simulated Cavity Measured with Digital Image Correlation
Published on: July 21, 2014
Fracture resistance of premolar screw-retained implant-supported hybrid abutment crowns with monolithic restorations
Junichi Honda1,2, Ryoki Takano3, Takuma Saito1
1Department of Fixed Prosthodontics, Nihon University School of Dentistry, Chiyoda-Ku, Tokyo, Japan.
Purpose:
This study evaluated the fracture resistance of premolar screw-retained implant-supported hybrid abutment crowns (HACs) fabricated from different monolithic restorative materials following artificial aging.
Materials And Methods:
Forty-four titanium implant analogs were restored with HACs fabricated from four materials: 5 mol% yttria-partially stabilized monolithic zirconia (ST), strength-gradient multilayered zirconia (YM), lithium disilicate ceramic (LD), and resin composite containing dispersed nanoparticles (CM) (n = 11 per group). All specimens were subjected to thermocycling (10,000 cycles) and mechanical loading (1.2 million cycles) to simulate 5 years of clinical service. Fracture resistance was evaluated under compressive loading, and failure modes were analyzed using optical microscopy and scanning electron microscopy. Statistical analysis was performed using the Kruskal-Wallis and Steel-Dwass tests (α = 0.05).
Results:
Significant differences were found among all groups (P = 0.00033-0.0022). The YM group exhibited the highest median fracture resistance (2.06 kN, IQR: 2.00 - 2.60 kN), followed by ST (1.74 kN, IQR: 1.69 - 1.80 kN), LD (1.29 kN, IQR: 1.14 - 1.41 kN), and CM (0.87 kN, IQR: 0.79 - 0.92 kN). All specimens survived the artificial aging protocols. Distinct fracture patterns were observed depending on the restorative material, with zirconia-based groups showing more favorable resistance than resin composite.
Conclusion:
All tested HACs exhibited fracture resistance values exceeding maximum bite forces, supporting their clinical applicability. Strength-gradient multilayered zirconia demonstrated superior reliability after simulated 5-year aging, emphasizing its structural advantage and broader safety margin compared with other restorative materials.
More Related Videos
Related Concept Videos
Fixing Double-strand Breaks
Fractures: Bone Repair
Minor fractures with no bone displacement are treated by immobilizing the fractured bone using a cast or splint. However, in the case of fractures with displaced bones, the broken bones are repositioned before immobilization to ensure successful healing without deformation and loss of function. The realignment of fractured bone ends is performed through a process called reduction. If the procedure...
Normal Strain under Axial Loading
Residual Stresses
Residual Stresses in Circular Shafts
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...