Microstructural Characterization of Defects and Secondary Phases in (Ti, Ta)C-Type Carbides in Nickel-Based
Xin Jin1, Yunsong Zhao2, Wei Chen1
1State Key Laboratory of Opto-Electronic Information Acquisition and Protection Technology, Leibniz International Joint Research Center of Materials Sciences of Anhui Province, Institutes of Physical Science and Information Technology, Anhui University, Hefei 230601, China.
Abstract:
Metal carbides (MCs) serve as essential strengthening phases in nickel-based superalloys, so the decomposition of MCs during high-temperature creep is regarded as detrimental to the mechanical properties and service life of these alloys. However, detailed investigations of the MC decomposition process at the microscale remain limited. In this study, the microstructure of MCs (where M is a mixture of Ti and Ta) in a nickel-based superalloy was characterized using aberration-corrected scanning transmission electron microscopy. The MCs exhibit a spherical core-shell structure, with Ta enrichment in the shell and Ti segregation in the core. Moreover, a high density of Cr-rich stacking faults, accompanied by Cr-rich M23C6 precipitates at their terminations, was identified in the Ti-rich cores, suggesting that these defects may be closely associated with the decomposition of MCs. This study may further expand the fundamental understanding of the interactions between defects and carbide properties.
More Related Videos
09:13Characterization of Ultra-fine Grained and Nanocrystalline Materials Using Transmission Kikuchi Diffraction
Published on: April 1, 2017
12:18Co-localizing Kelvin Probe Force Microscopy with Other Microscopies and Spectroscopies: Selected Applications in Corrosion Characterization of Alloys
Published on: June 27, 2022
Related Concept Videos
Imperfections in Crystal Structure: Non-Stoichiometric Defects
Imperfections in Crystal Structure: Stoichiometric Point Defects