Physical and surface analysis of calcium silicate Clinker after acid challenge: a micro-CT and SEM study
Karina Ines Medina Carita Tavares1, Airton Oliveira Santos-Junior1, Jáder Camilo Pinto2
1Universidade Estadual Paulista - Unesp, School of Dentistry, Department of Restorative Dentistry, Araraquara, SP, Brazil.
Abstract:
The purpose of this study was to evaluate the effect of immersion in butyric acid (BA, pH 4.1) or phosphate-buffered saline (PBS, pH 7.0) on the properties of Clinker (CL) with particle sizes of 2 to 30 µm or < 2 µm associated with zirconium oxide and manipulated with distilled water (DW) or liquid with additives (LA) compared with Bio-C Repair (BCR) and Biodentine (BIO). Dentin tubes were prepared and filled with materials. After 24 hours, the specimens were immersed in BA or PBS (n = 5) for 7 and 28 days. Micro-computed tomography was used to evaluate volumetric change, porosity, and material/dentin interface. Surface analysis was performed by scanning electron microscopy (SEM). Statistical analyses included Kruskal-Wallis and Dunn, Mann-Whitney, Wilcoxon, unpaired t-test, paired t-test, and ANOVA and Tukey tests (α = 0.05). All groups exhibited volumetric changes similar to BCR and BIO (p > 0.05). BA significantly increased porosity (approximately 8%) compared with PBS (approximately 2%), except for CL 2 to 30 µm with LA (p < 0.05). After 28 days in BA, all groups showed increased porosity and gaps at the interface compared with baseline values (p < 0.05). CL 2 to 30 µm with DW showed greater porosity and interface gaps than the other groups (p < 0.05). SEM analysis revealed that all groups showed hydroxyapatite formation on the material surface in PBS, and structural loss in BA. Findings: Acidic pH damages the material/dentin interface, increases porosity, and promotes dimensional changes in calcium silicate cements. Distilled water without additives increases the Clinker's porosity, interface gaps, and volume loss.
Related Concept Videos
Hydration of Cement
Sulfate Attack on Concrete
Sulfates from sources like soil, groundwater, or industrial effluents...
Soundness of Cement
Microcracking in Concrete
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Acid Attack on Concrete
The rate at which hydrogen...