Prediction model for compressive strength of alkali-activated multi-source solid-waste grouting materials based on
Qiang Yue1, Guangming Yu2, Yong Yao1
1China Construction Fifth Engineering Bureau Co., Ltd., Changsha, Hunan, China.
Abstract:
Alkali-activated multi-source solid-waste grouting materials have attracted increasing attention in geotechnical and underground engineering due to their low carbon footprint, environmental friendliness, and potential for large-scale resource utilization. However, the complex composition and multiple influencing factors of these materials pose significant challenges for understanding and predicting their compressive strength, particularly under conditions characterized by small sample sizes, high-dimensional variables, and strong nonlinearity. To address these issues, an experimental database comprising 179 UCS records compiled from three independent experimental studies was established. Fifteen experimental records were reserved for external validation, while WGAN-GP was trained using the remaining 164 model-development samples, thereby keeping the external validation set completely isolated from model development. Multiple machine learning models were then developed to establish a UCS prediction framework. Furthermore, the Newton-Raphson-Based Optimizer (NRBO) was applied to optimize the hyperparameters of the XGBoost model, resulting in an NRBO-XGBoost prediction model. The SHAP method was introduced to interpret the prediction results and quantify the contribution of each input variable. The results demonstrate that WGAN-GP effectively preserves the statistical characteristics and inter-variable correlations of the original data, thereby improving model-training stability and generalization performance. Among all models considered, NRBO-XGBoost exhibited the best predictive performance, achieving an R2 of 0.964, an RMSE of 3.411 MPa, and an MAE of 2.474 MPa in the testing phase. SHAP analysis further revealed that cement content, water-to-binder ratio, curing age, alkali equivalent, and ground granulated blast-furnace slag content play dominant roles in governing compressive strength development. The integrated framework of data augmentation, optimized modeling, and interpretable analysis proposed in this study provides reliable data-driven decision support for mix design optimization and engineering application of alkali-activated multi-source solid-waste grouting materials, and offers a novel technical pathway for performance prediction of complex cementitious materials.
Related Concept Videos
Alkali Aggregate Reaction in Concrete
Bonding and Strength of Aggregate
Mortar Properties
Design Example: Aggregate Gradation
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is sampled...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Pozzolans
Fly ash is a...