Comparison of the root-end sealing ability of MTA and Portland cement
Intekhab Islam1, Hui Kheng Chng, Adrian U Jin Yap
1Department of Restoraive Dentistry, Faculty of Dentistry, National University of Singapore, 5 Lower Kent Ridge Road, Singapore 119074, Singapore.
Abstract:
The aim of this study was to compare the in vitro sealing ability of ProRoot MTA, ProRoot MTA (Tooth-Coloured Formula), ordinary Portland cement and white Portland cement when used as root-end filling materials. Twenty-four single-rooted human premolars were prepared and obturated using standard techniques, then retrofilled with the test materials. The prepared teeth were immersed in 1% methylene blue dye for 72 hours and then assessed for dye leakage. The depth of dye penetration was measured and expressed as a percentage of the length of the retrofilling. Data was analysed using ANOVA and Fisher's Least Significant Test (LSD) (p < 0.05). None of the teeth in any of the test groups showed leakage beyond the retrofillings. Given the low cost and apparently similar sealing ability of the cements, it is reasonable to consider Portland cement as a possible substitute for MTA as a root-end filling material. However, further tests, especially in vivo biocompatibility tests, need to be conducted before Portland cement can be recommended for clinical use.
Related Concept Videos
Types of Cement II
Mortar Properties
Mortar
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Testing Water Quality
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...