Related Experiment Video
Updated: May 21, 2026

Fabrication And Characterization Of Photonic Crystal Slow Light Waveguides And Cavities
Published on: November 30, 2012
Thickness dependence of amplified spontaneous emission in low-absorbing organic waveguides
Eva M Calzado1, Manuel G Ramírez, Pedro G Boj
1Instituto Universitario de Materiales de Alicante (IUMA) and Unidad Asociada UA-CSIC, Universidad de Alicante, 03080-Alicante, Spain.
Abstract:
The effect of varying film thickness (h) on the amplified spontaneous emission (ASE) properties of 0.5 wt.% perylenediimide-doped polystyrene waveguides is reported. The threshold dependence on h, not previously investigated in detail, is analyzed in terms of the film absorption and photoluminescence, the confinement of the fundamental waveguide mode (TE0), and the presence of high-order modes. For h<400 nm and down to 150 nm, the ASE wavelength blueshifts, while the linewidth and threshold increase. The detrimental ASE operation in very thin films is due to the low absorption as well as to the poor confinement of the TE0 mode.
Related Concept Videos
UV–Vis Spectroscopy: Beer–Lambert Law
UV–Vis Spectroscopy of Conjugated Systems
One of the factors influencing λmax is the extent of conjugation in the...
UV–Vis Spectrum
The UV–Vis spectrum of a molecule is the plot of its absorbance versus wavelength. The plot is drawn by taking molar absorptivity (ε) or log ε on the y-axis (ordinate)...
Molecular Spectroscopy: Absorption and Emission