Correlative fractography: combining scanning electron microscopy and light microscopes for qualitative and
Luis Rogerio de Oliveira Hein1, José Alberto de Oliveira, Kamila Amato de Campos
1UNESP-Univ Estadual Paulista, DMT-Department of Materials and Technology, LAIMat-Materials Imaging Laboratory, Av. Ariberto Pereira da Cunha, 333, Guaratinguetá, SP, 12.516-410, Brazil. rhein@feg.unesp.br
Abstract:
Correlative fractography is a new expression proposed here to describe a new method for the association between scanning electron microscopy (SEM) and light microscopy (LM) for the qualitative and quantitative analysis of fracture surfaces. This article presents a new method involving the fusion of one elevation map obtained by extended depth from focus reconstruction from LM with exactly the same area by SEM and associated techniques, as X-ray mapping. The true topographic information is perfectly associated to local fracture mechanisms with this new technique, presented here as an alternative to stereo-pair reconstruction for the investigation of fractured components. The great advantage of this technique resides in the possibility of combining any imaging methods associated with LM and SEM for the same observed field from fracture surface.
More Related Videos
12:18Co-localizing Kelvin Probe Force Microscopy with Other Microscopies and Spectroscopies: Selected Applications in Corrosion Characterization of Alloys
Published on: June 27, 2022
09:34A Method to Estimate Cadaveric Femur Cortical Strains During Fracture Testing Using Digital Image Correlation
Published on: September 14, 2017
Related Concept Videos
Scanning Electron Microscopy
Fundamental Principles
Accelerated...
Confocal Fluorescence Microscopy
Atomic Force Microscopy
The AFM Probe
The probe is regarded as the heart of any AFM setup and comprises the...
Overview of Microscopy Techniques
Electron Microscope Tomography and Single-particle Reconstruction
Electron Tomography
Electron tomography can be performed either in TEM or STEM (scanning transmission...
Three-Dimensional Microscopy in Microbiology