Self-assembled Ni/TiO2 nanocomposite anodes synthesized via electroless plating and atomic layer deposition on
Konstantinos Gerasopoulos1, Xilin Chen, James Culver
1MEMS Sensors and Actuators Laboratory, Department of Materials Science and Engineering, Institute for Systems Research, University of Maryland, 2173 A.V. Williams Building, College Park, MD 20742, USA.
Abstract:
Ni(core)/TiO(2)(shell) nanocomposite anodes were fabricated on three-dimensional, self-assembled nanotemplates of Tobacco mosaic virus using atomic layer deposition, exhibiting high capacities and rate capability and extremely low average capacity fading (∼0.024% per cycle) for ∼1000 cycles.