Preparation of Large-area Vertical 2D Crystal Hetero-structures Through the Sulfurization of Transition Metal Films for Device Fabrication
Published on: November 28, 2017
MoS2 thin films from a (N t Bu)2(NMe2)2Mo and 1-propanethiol atomic layer deposition process
Berc Kalanyan1, Ryan Beams1, Michael B Katz1
1Material Measurement Laboratory, National Institute of Standards and Technology, Gaithersburg, Maryland 20899.
Abstract:
Potential commercial applications for transition metal dichalcogenide (TMD) semiconductors such as MoS2 rely on unique material properties that are only accessible at monolayer to few-layer thickness regimes. Therefore, production methods that lend themselves to scalable and controllable formation of TMD films on surfaces are desirable for high volume manufacturing of devices based on these materials. We have developed a new thermal atomic layer deposition (ALD) process using bis(tert-butylimido)-bis(dimethylamido)molybdenum and 1-propanethiol to produce MoS2-containing amorphous films. We observe self-limiting reaction behavior with respect to both the Mo and S precursors at a substrate temperature of 350 °C. Film thickness scales linearly with precursor cycling, with growth per cycle values of ≈0.1 nm/cycle. As-deposited films are smooth and contain nitrogen and carbon impurities attributed to poor ligand elimination from the Mo source. Upon high-temperature annealing, a large portion of the impurities are removed, and we obtain few-layer crystalline 2H-MoS2 films.
More Related Videos
06:00Solvothermal Synthesis of MIL-96 and UiO-66-NH2 on Atomic Layer Deposited Metal Oxide Coatings on Fiber Mats
Published on: June 13, 2018
08:12Ohmic Contact Fabrication Using a Focused-ion Beam Technique and Electrical Characterization for Layer Semiconductor Nanostructures
Published on: December 5, 2015